The top pic shows the chassis completely stripped and washed with AQUA CLEAN by KBS Coatings. It is a three part system. The second part of the system is washing down in a product called RUST BLAST, it is a self-etching primer that also neutralises the rust. The white film you can see is the zinc cozting that is applied over the metal to protect it for upto 30 days prior to painting. The final coat will be RUST SEAL which bonds to teh steal and creates a incredibly hard surface, in gloss black.
So to apply the RUST SEAL It needs to be below 28 degrees and 60% humidity!!!! And that just aint happening here in Rainy QLD where it rains more than Melbourne!! Its either below 60% humidity and 30+ degrees or 25 degrees and 85% humidity! Cant win...only got max of 30 days before I'll have to recoat with RUST BLAST!